The mixed metal oxides are formed on the substrate through a process of thermal- decomposition, creating an oxide coating of the platinum group metals. The oxide coatings have many the superior performances, such as
Lightweight
MMO coatings demonstrate very high chemical stability even in environments with very low PH values
The coating is not affected by the generation of chlorine
The wear rate of the anode is extremely low and uniform and between 1 and 6 milligrams/ampere-year.
The anode dimensions remain nearly constant during the design life.
Operated at high current density, 2000A/m2.
The superior electrically-conductive performance: 10-7ฮฉยทm